Por favor, use este identificador para citar o enlazar este ítem: http://repositorio.ufc.br/handle/riufc/67470
Tipo: Artigo de Periódico
Título : Rapid Sonochemical Approach Produces Functionalized Fe3O4 Nanoparticles with Excellent Magnetic, Colloidal, and Relaxivity Properties for MRI Application
Autor : Andrade Neto, Davino Machado
Freire, Rafael Melo
Gallo, Juan
Freire, Tiago Melo
Queiroz, Danilo Caldas de
Ricardo, Nágila Maria Pontes Silva
Vasconcelos, Igor Frota de
Mele, Giuseppe Agostino
Carbone, Luigi
Mazzetto, Selma Elaine
Bañobre-López, Manuel
Fechine, Pierre Basílio Almeida
Palabras clave : Functionalization;Imaging agents;Molecules;Nanoparticles;Physical and Chemical processes
Fecha de publicación : 2017
Editorial : The Journal of Physical Chemistry C
Citación : ANDRADE NETO, Davino Machado et al. Rapid sonochemical approach produces functionalized Fe3O4 Nanoparticles with excellent magnetic, colloidal, and relaxivity properties for MRI application. The Journal of Physical Chemistry C, [s. l.], v. 121, n. 43, p. 24206-24222, 2017.
Abstract: Functionalized Fe3O4 nanoparticles (NPs) have emerged as a promising contrast agent for magnetic resonance imaging (MRI). Their synthesis and functionalization methodology strongly affect their performance in vivo. The methodology most used in the literature for the synthesis of Fe3O4 NPs is thermal decomposition, which has proven to be time-consuming, expensive, and laborious, as it requires further ligand exchange strategies to transfer the as-synthesized nanoparticles from organic to aqueous solvents. This work describes a rapid and facile sonochemical methodology to synthesize and functionalize Fe3O4 NPs with excellent physicochemical properties for MRI. This sonochemistry approach was used to produce, in 12 min, Fe3O4 NPs functionalized with polysodium acrylate (PAANa), trisodium citrate (CIT), branched polyethylenimine (BPEI), and sodium oleate. X-ray diffraction and transmission electron microscopy demonstrated that the NPs were composed of a single inverse spinel phase with an average diameter of 9–11 nm and a narrow size distribution. Mössbauer spectroscopy and magnetic measurements confirmed that the obtained NPs were transitioning to the superparamagnetic regime and possessed excellent magnetization saturation values (59–77 emu/g). Fourier transform infrared spectroscopy proved that the sonochemistry approach provided conditions that induced a strong interaction between Fe3O4 and the coating agents. Furthermore, dynamic light-scattering experiments evidenced that samples coated with PAANa, CIT, and BPEI possess colloidal stability in aqueous solvents. Emphasis must be placed on PAANa-coated NPs, which also presented remarkable colloidal stability under simulated physiological conditions. Finally, the obtained NPs exhibited great potential to be applied as an MRI contrast agent. The transverse relaxivity values of the NPs synthesized in this work (277–439 mM–1 s–1) were greater than those of commercial NPs and those prepared using other methodologies. Therefore, this work represents significant progress in the preparation of Fe3O4 NPs, providing a method to prepare high-quality materials in a rapid, cost-effective, and facile manner.
URI : http://www.repositorio.ufc.br/handle/riufc/67470
ISSN : 1932-7455
Aparece en las colecciones: DEMM - Artigos publicados em revista científica

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
2017_art_dmandradeneto.pdf8,78 MBAdobe PDFVisualizar/Abrir


Los ítems de DSpace están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.