Tipo: | Artigo de Periódico |
Título: | Debris extrusion and foraminal deformation produced by reciprocating instruments made of thermally treated NiTi wires |
Autor(es): | Frota, Myrna Maria Arcanjo Bernardes, Ricardo Affonso Vivan, Rodrigo Ricci Vivacqua-Gomes, Nilton Duarte, Marco Antonio Hungaro Vasconcelos, Bruno Carvalho de |
Palavras-chave: | Endodontia;Endodontics;Titânio;Cavidade Pulpar;Dental Pulp Cavity |
Data do documento: | Jan-2018 |
Instituição/Editor/Publicador: | Journal of Applied Oral Science |
Citação: | FROTA, M. M. A. et al. Debris extrusion and foraminal deformation produced by reciprocating instruments made of thermally treated NiTi wires. Journal of Applied Oral Science, Bauru, e20170215, jan. 2018. |
Abstract: | Objective: To evaluate the amount of apically extruded debris, percentage of foraminal enlargement and apical foramen (AF) deformation that occurred during root canal preparation with different reciprocation systems: Reciproc, WaveOne (M-Wire), and ProDesign R (Shape Memory Technology Wire) at two different working lengths (WLs): 0.0 and 1.0 mm beyond the AF. Material and methods: The AF of 120 root canals in 60 mesial roots of mandibular molars were photographed with stereomicroscope and randomly assigned into four groups: manual, Reciproc (REC), WaveOne (WO), and ProDesign R (PDR); subsequently, they were further subdivided according to the WL (n=15). Teeth were instrumented, coupled to a dual collecting chamber, and then another photograph of each AF was captured. Extrusion was analysed by determining the weight of extruded debris. Each AF diameter was measured in pre- and post-instrumentation images to determine deformation, which was analysed, and afterwards the final format of AFs was classified (circular/oval/deformed). Results: We found no significant differences when analysing each system at different WLs. When considering each WL, REC and WO showed highest extrusion values (P<.05); for AF enlargement, differences were observed only for WO, when it was used beyond the AF; differences were observed among M-Wire groups beyond the AF (P<.05). AF deformation was observed in all groups; PDR showed the lowest AF deformation values at both WLs; M-Wire groups showed 50% strain beyond the AF. Conclusion: Authors concluded that beyond the apical limit, the alloy and taper are important aspects when considering extrusion and deformation. |
URI: | http://www.repositorio.ufc.br/handle/riufc/40088 |
ISSN: | 1678-7765 On-line |
Aparece nas coleções: | DCOD - Artigos publicados em revistas científicas |
Arquivos associados a este item:
Arquivo | Descrição | Tamanho | Formato | |
---|---|---|---|---|
2018-art_mmarcanjo.pdf | 492,87 kB | Adobe PDF | Visualizar/Abrir |
Os itens no repositório estão protegidos por copyright, com todos os direitos reservados, salvo quando é indicado o contrário.