dc.contributor.authorRibeiro, Thiago Soares-
dc.contributor.authorSasaki, José Marcos-
dc.contributor.authorVasconcelos, Igor Frota de-
dc.date.accessioned2022-08-10T16:26:54Z-
dc.date.available2022-08-10T16:26:54Z-
dc.date.issued2012-
dc.identifier.citationRIBEIRO, Thiago Soares; SASAKI, José Marcos; VASCONCELOS, Igor Frota de. Structural disorder of ball-milled, nanosized, Fe-doped SnO2: X-ray diffraction and Mössbauer spectroscopy characterization. Journal of Materials Science, [s. l.], v. 47, p. 2630-2636, 2012.pt_BR
dc.identifier.issn1573-4803-
dc.identifier.urihttp://www.repositorio.ufc.br/handle/riufc/67658-
dc.description.abstractStructural characterization of nanosized Fe-doped semiconducting oxide SnO2 is reported. Samples of Sn1−x Fe x O2−y (with x ranging from 0.11 to 0.33) were processed in a planetary ball mill, subsequently HCl-washed to eliminate metallic iron impurities introduced by the milling tools, and characterized by X-ray diffraction and Mössbauer spectroscopy. Results showed that Fe enters the host matrix randomly replacing Sn in octahedral sites regardless of iron concentration. It has been found the presence of oxygen deficient iron sites attributed to the stoichiometric unbalance of precursor materials used in the milling process. It is known that structural features like particle size and residual microstrain are highly affected by the milling process. Values of average particle sizes as calculated by Scherrer’s method alone decreased with increasing Fe concentration. This result was shown, by means of the Williamson-Hall correction method, to be misleading as a large degree of microstrain is expected for mechanically milled powders. In fact, corrected values of average particle sizes turned out to be reasonably homogeneous regardless of iron content and milling time with no consistent trend. Residual microstrain, on the other hand, was found to increase with iron content giving way to the conclusion that broadening of diffraction peaks are mostly due to increasing microstrain as a function of iron doping and milling time. Williamson-Hall analysis also showed a large degree of particle size inhomogeneity. Milling of undoped SnO2 showed that this inhomogeneity is due mostly to doping as opposed to milling.pt_BR
dc.language.isoenpt_BR
dc.publisherJournal of Materials Sciencept_BR
dc.subjectMillingpt_BR
dc.subjectSnO2pt_BR
dc.subjectAverage particle sizept_BR
dc.subjectQuadrupole splittingpt_BR
dc.subjectMilling timept_BR
dc.titleStructural disorder of ball-milled, nanosized, Fe-doped SnO2: X-ray diffraction and Mössbauer spectroscopy characterizationpt_BR
dc.typeArtigo de Periódicopt_BR
Aparece nas coleções:DEMM - Artigos publicados em revista científica

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
2012_art_tsribeiro.pdf2,22 MBAdobe PDFVisualizar/Abrir


Os itens no repositório estão protegidos por copyright, com todos os direitos reservados, salvo quando é indicado o contrário.