dc.contributor.authorFlórez, Mauro Andrés Cerra-
dc.contributor.authorRibas, Gemma Fargas-
dc.contributor.authorRovira, Joan Josep Roa-
dc.contributor.authorGarcía, Antonio Manuel Mateo-
dc.contributor.authorMata, Stephany Aparecida Santos da-
dc.contributor.authorRodríguez-Castellón, Enrique-
dc.contributor.authorSilva, Marcelo José Gomes da-
dc.date.accessioned2022-08-19T13:57:27Z-
dc.date.available2022-08-19T13:57:27Z-
dc.date.issued2022-
dc.identifier.citationFLOREZ, Mauro Andres Cerra et al. Synthesis and characterization of an Fe/Co ferrite spinel oxide film produced by using N2/steam heat treatment on two maraging steels. Metallurgical and Materials Transactions A, [s. l.], v. 53, p. 1276-1293, 2022.pt_BR
dc.identifier.issn1543-1940-
dc.identifier.urihttp://www.repositorio.ufc.br/handle/riufc/67780-
dc.description.abstractAn experimental procedure was developed to obtain an oxide layer formed mainly by spinel on maraging steels. It consists of different stages with specific conditions, such as atmospheres rich in nitrogen and water vapor, and different steps of temperatures and times. Tests were performed on grade 300 and 350 maraging steels. Oxide layer characterization was done using optical and electron microscopy, spectroscopy, X-ray diffraction, and nanoscratch tests in order to determine the adhesion force as well as to observe the main deformation mechanism induced under sliding tests. In both steels, oxide layers are formed by the spinel’s Fe3O4 and CoFe2O4 in amounts close to ca. 85 pct, whereas TiO2 and MoO3 represent the other 15 pct. No hematite was found. The low oxygen availability during the heat treatment was fundamental for avoiding hematite formation. A nickel-rich austenitic phase formed at the metal-oxide interface due the kinetics of the oxidation process of the cobalt, iron, and molybdenum. The particular conditions of the heat treatments induced the formation of a mixture of iron, nickel, and cobalt spinel ferrites, thereby contradicting previous studies that said that only magnetite would be formed. The sliding tests at the nanometric length scale highlight that the layer formed on maraging 300 grade presents a better adhesion than the other investigated material due to the fact that it requires more load in order to induce cracks located at the edge of the sliding track and, subsequently, the chipping of the formed layer.pt_BR
dc.language.isoenpt_BR
dc.publisherMetallurgical and Materials Transactions Apt_BR
dc.subjectFerrite Fe/Copt_BR
dc.subjectMaraging steelspt_BR
dc.subjectSteam condensationpt_BR
dc.titleSynthesis and characterization of an Fe/Co ferrite spinel oxide film produced by using N2/steam heat treatment on two maraging steelspt_BR
dc.typeArtigo de Periódicopt_BR
Aparece nas coleções:DEMM - Artigos publicados em revista científica

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
2022_art_macflores.pdf9,5 MBAdobe PDFVisualizar/Abrir


Os itens no repositório estão protegidos por copyright, com todos os direitos reservados, salvo quando é indicado o contrário.